Title: Research Needs for HPC-An Australian Perspective

Author(s): W. G. Ryan and R. J. Potter

Publication: Symposium Paper

Volume: 159

Issue:

Appears on pages(s): 105-116

Keywords: Curing; durability; fire resistance; high-performance concretes;lightweight concretes; research

DOI: 10.14359/10051

Date: 2/1/1996

Abstract:
Australia is a dry warm continent. The major population centres are located close to the coastline. This paper examines the predictions for future building and construction activity in Australia. Based on the physical situation, for example climate and geography, and the anticipated needs for HPC arising from the forecast trends in construction activity it tries to forecast the research needs for HPC in Australia. It also endeavours to assign priorities for these research needs in terms of the size of the market likely to be affected.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer