International Concrete Abstracts Portal

  


Title: Influence of Slag Cement on the Water Sorptivity of Concrete

Author(s): D. W. S. Ho, I. Hinczak, J. J. Conroy, and R. K. Lewis

Publication: Symposium Paper

Volume: 91

Issue:

Appears on pages(s): 1463-1474

Keywords: blast furnace slag; concrete durability; curing; portland slag cements; sorption; water; wetting and drying tests.

DOI: 10.14359/10131

Date: 2/1/1986

Abstract:
This paper explains the concept of water sorptivity as a measure of concrete quality and discusses the effect of interrupted curing (as distinct from continuous curing) on the quality of concrete. Results of a pilot study on concretes incorporating ground granulated blast-furnace slag either as a blend or as an intergrind are presented. It was found that the response to interrupted curing varied depending on the constituents of the concrete. Plain concrete (i.e. without chemical or mineral admixtures) with a 28-day strength of 28 MPa showed a very slow response to interrupted curing, but could be improved by the incorporation of slag or by specifying a higher 28-day strength.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.