Title: Durability of Reactive Powder Concrete When Subjected to a leaching Test

Author(s): V. Matte, M. Cheyrezy, M. Moranville, C. Richet, and J-M Torrenti

Publication: Symposium Paper

Volume: 200

Issue:

Appears on pages(s): 433-446

Keywords: diffusion; leaching; microstructure; mineralogy; porosity; reactive powder concrete

DOI: 10.14359/10593

Date: 6/1/2001

Abstract:
The Reactive Powder Concretes (RPC) are well known for their high strength, but they also present good performances regarding durability aspect due to their very dense microstructure. Studies were made to evaluate the durability of RPC to : freeze-thaw scaling, carbonation, chloride ions diffusion, abrasion coefficient and shrinkage. Their very good performance characteristics have led to a specific research programme to evaluate the long-term durability of RPC for nuclear waste containment. Several kinds of potential degradation are studied, but here only the attack by de-ionised water, a very severe leaching test, will be presented. After pre-determined periods, the material was analysed regarding its microstructure (altered depth, composition and mineralogical changes), porosity and ion transport properties. The results of SEM, X-Ray diffraction, mercury intrusion porosimetry, BET pore-size and tritium diffusion coefficient analyses are presented.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer