International Concrete Abstracts Portal

  


Title: State of the Art Report on High-Strength Concrete

Author(s): ACI Committee 363

Publication: Journal Proceedings

Volume: 81

Issue: 4

Appears on pages(s): 364-411

Keywords: bibliographies; bridges (structures); buildings; conveying; economics; high-strength concretes; mechanical properties; mixing; mix proportioning; placing; quality control; raw materials; reviews; structural design.

DOI: 10.14359/10692

Date: 7/1/1984

Abstract:
Currently available information about high-strength concrete is summarized. Topics discussed include selection materials, concrete mix proportioning, batching, mixing, transporting, placing, control procedures, concrete properties, structural design, economics, and applications. A bibliography is included.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.