Title: Staggered Shear Design of Simply Supported Concrete Beams

Author(s): Peter Marti

Publication: Journal Proceedings

Volume: 83

Issue: 1

Appears on pages(s): 36-42

Keywords: beams (supports); girders; limit design method; loads (forces); reinforced concrete; reinforcing steels; shear strength; structural analysis.

DOI: 10.14359/10740

Date: 1/1/1986

Abstract:
The staggering concept of shear design is shown to be valid for simply supported beams subjected to uniformly distributed and moving concentrated or truck loads applied at the top. Two design examples illustrate the application of the staggering concept to beams carrying uniformly distributed loads and moving trucks.




  