Title: 
            Stress-Strain Response and Fracture of
Concrete in Biaxial Loading
        
        
            Author(s): 
            M. Ebrahim Tasuji, Floyd 0. Slate, and Arthur H. Nilson
        
        
            
                Publication: 
                Journal Proceedings
            
            
                Volume: 
                75
            
            
                Issue: 
                7
            
            
                Appears on pages(s): 
                306-312
            
            
                Keywords: 
                biaxial loads; compressive strength: concretes;deformation; failure mechanisms; microcracking; strains;stress-strain relationships; tensile properties; tensile strength.
            
            
                DOI: 
                10.14359/10944
            
        
        
            Date: 
            7/1/1978
        
        
            Abstract:
            Thin plain concrete plates subject to biaxial loading were studied experimentally. All combinations of compressive and tensile loadings were included.  Deformational characteristics, fracture mechanism, and strength were observed.  Results confirm that concrete possesses higher strength in biaxial compression than in uniaxial compression.  Under combined compression and tension, the compressive strength decreases almost linearly as the tensile stress increases. The biaxial tensile strength of concrete is greater than its uniaxial tensile strength. Observed modes of failure and measurements of tensile deformation enforce the idea that the most appropriate concrete failure criterion, for uniaxial and biaxial states of stress, is limiting tensile strain. The magnitude of the limiting tensile strain decreases with the degree of direct tensile loading involved and increases with the degree of compression.  A general stress-strain relationship for concrete in biaxial loading is proposed. In addition, a simple biaxial strength criterion is recommended for practical application.