Title: Recommended Practice for Curing Concrete (AC1 308-71)

Author(s): ACI Committee 308

Publication: Journal Proceedings

Volume: 69

Issue: 1

Appears on pages(s): 1

Keywords: bridges (structures); buildings; cement base paints;. cold weather construc- tion; concrete construction; concrete pavements; concretes; curing; curing compounds;curing films and sheets; hot weather construction: insulating concrete; insulation.

DOI: 10.14359/11244

Date: 1/1/1972

Abstract:
Curing is defined as the process of maintaining a satisfactory moisture content and a favorable temperature in concrete during hydration of the cementitious materials so that desired properties of the concrete are developed. Two systems of providing the required moisture are explained in detail: (I) main-taining a moist environment by application of water; and (2) prevention of IOSS of mixing water by use of sealing materials. Basic principles of successful curing are outlined, and commonly accepted methods, procedures, and materials are described. Recommendations are given for curing pavements and other slabs on ground; for structures and buildings: and for mass concrete. For each of these categories, methods, materials, time and temperature of curing are recommended. Brief sections comment on curing requirements for precast products, shotcrete, preplaced aggregate concrete, refractory concrete, plaster and other applications.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer