Title: Concrete Damage as a Fatigue Phenomenon

Author(s): C. Meyer

Publication: Symposium Paper

Volume: 205

Issue:

Appears on pages(s): 347-366

Keywords: cyclic loads; fatigue; stiffness degradation; strength

DOI: 10.14359/11647

Date: 1/1/2002

Abstract:
When designing concrete structures, fatigue related problems are not among the first that come to mind. However, structures subjected to strong cyclic loads such as those associated with destructive earthquakes experience strength and stiffness degradation that are most aptly described as a low-cycle fatigue phenomenon and are related to the damage accumulated under such loading. This paper briefly discusses the various elements of a rational, i.e. mechanics-based design methodology. Results of an experimental test program are summarized, in which 4-inch cubes with or without fiber reinforcement are subjected to uni- and biaxial cyclic compression until failure. The review concludes with a brief review of the various aspects of material behavior that need to be modeled, if the response of reinforced concrete members is to be simulated numerically.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer