Title: Design of Prismatic Shells

Author(s): Hermann Craemer

Publication: Journal Proceedings

Volume: 49

Issue: 2

Appears on pages(s): 549-563

Keywords: no keywords

DOI: 10.14359/11836

Date: 2/1/1953

Abstract:
Differential equations for prismatic shells, based on the deflections of the edges, are derived and integrated for several single-span systems of various cross-sectional types. Depending on the cross section and the span, there is a gradual transition from a pure shell effect to that of a thin-walled beam.




  