Title: The Ultimate Strength of Reinforced Concrete Beams

Author(s): S. D. Lash and J. W. Brison

Publication: Journal Proceedings

Volume: 46

Issue: 2

Appears on pages(s): 457-470

Keywords: no keywords

DOI: 10.14359/12068

Date: 2/1/1950

Abstract:
The results of tests to failures on 57 small reinforced concrete beams are presented, and it is shown that they can be explained satisfactorily on the basis of a simple plastic theory of design. Formulas are proposed for determining the moments of resistance and the critical percentages of reinforcement.




  