Title: Prestressed beam

Author(s): Adolfo Matamoros and Julio A. Ramirez

Publication: Symposium Paper

Volume: 208

Issue:

Appears on pages(s): 163-184

Keywords:

DOI: 10.14359/12419

Date: 10/29/2002

Abstract:
The design of the end region of a prestressed beam according to Appendix A of the 2002 ACI Building Code is presented. Two alternatives are considered, the first with straight strands and debonding toward the ends of the member in order to control stresses at transfer. The second case is with draped strands. Strut-and-tie modles corresponding to each of the two alernatives are developed, analyzed, and the reinforcement is proportioned to reseist the calculated internal forces. Anchorage length requirements were a critical factor in selecting the configuration of the truss model.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer