Title: Extending the Life of Concrete Repairs

Author(s): Jay H. Paul

Publication: Concrete International

Volume: 20

Issue: 3

Appears on pages(s): 62-66

Keywords: contaminants; deterioration; protective coatings; repairs; surface coatings;

DOI:

Date: 3/1/1998

Abstract:
While the results of a repair program are easy for an owner to see, the benefits of a protection system may be a difficult sell. However, the primary reason for a protection system is to extend the life of the concrete repairs. By moderating the underlying causes of concrete deterioration, the performance of repairs will improve. An overview of various systems for protecting concrete is offered.




  