Behavior of Concrete liquid Containing Structures Subjected to Seismic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Concrete liquid Containing Structures Subjected to Seismic Loading

Author(s): M. R. Kianoush, W. K. Tso, and M. Hamidi

Publication: Symposium Paper

Volume: 209

Issue:

Appears on pages(s): 389-404

Keywords: circular tank; concrete; design code; earthquake; liquid containing; seismic; water retaining

DOI: 10.14359/12511

Date: 9/26/2002

Abstract:
The behavior of liquid containing structures (LCS) subjected to seismic excitations is reviewed. The major parameters affecting the response of concrete circular tanks for LCS are discussed. Existing codes aud standards related to seismic design of LCS are reviewed. With the aid of a design example, results of the various design standards are compared. The effects of earthquake load on the behavior of reinforced concrete (RC) tanks are also investigated through a detailed example.




  