Title: Evaluation of Creep and Shrinkage Deflections of Reinforced Concrete Members in the Current Australian Practice

Author(s): B. Vijaya Rangan

Publication: Symposium Paper

Volume: 129

Issue:

Appears on pages(s): 56-76

Keywords: creep properties; deflection; reinforced concrete; serviceability; shrinkage; structural design; Structural Research

DOI: 10.14359/1255

Date: 12/1/1991

Abstract:
The paper presents a summary of treatment of deflection control in the Australian Standard, AS3600-1988. The top-tier method recommended by the standard requires consideration of creep and shrinkage effects on deflections. Simple expressions for calculating creep and shrinkage deflections are given and illustrated by examples.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer