Flexural Stiffness of High Strength Concrete Beams Reinforced with GFRP Bars

International Concrete Abstracts Portal

  


Title: Flexural Stiffness of High Strength Concrete Beams Reinforced with GFRP Bars

Author(s): J. R. Yost, S. P. Gross, and D. W. Dinehart

Publication: Symposium Paper

Volume: 210

Issue:

Appears on pages(s): 209-224

Keywords: deflection; flexural stiffness; FRP; reinforced concrete beams

DOI: 10.14359/12580

Date: 2/1/2003

Abstract:
Deflection behavior of high strength concrete (HSC) flexural members reinforced with glass-fiber polymer bars (GFRP) is investigated. Because serviceability plays a significant role in establishing design acceptance for GFRP reinforced concrete beams, accurate modeling of flexural stiffness is critical and he effect of influencing parameters must be considered. This study accounts ofr variations in reinforcement ratio ( r ) for HSC beams. Experimental results from twelve simply supported concrete beams reinforced with GFRP bars are compared with published deflection models to establish analytic accuracy. All samples have a hear-span-to-depth ratio of 9.4 and are overreinforced with respect to a balanced strain design. Results show that the ACI 318 and ACI 440 effective moment-of-inertia expressions greatly overestimate flexural stiffnes, with the degree of inaccuracy dependent upon on reinforcement ratio.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer