Title: Design Guidelines for Anchorage to Concrete

Author(s): H. Wiewel

Publication: Symposium Paper

Volume: 130

Issue:

Appears on pages(s): 1-18

Keywords: anchors (fasteners); shear strength; tensile strength; tension; working stress method; Structural Research

DOI: 10.14359/1265

Date: 1/1/1992

Abstract:
Design information for concrete anchors is summarized in this paper. Based on recent research, the tension and shear capacities published in the past for concrete anchors are generally unconservative, especially data for proprietary concrete anchors. This paper recommends new design parameters for seven categories of concrete anchors. The parameters, presented in tabular form, are related to tension zone cracking and seismic loading, as well as spacing and edge distance.




  