Lateral Blow out Failure of Headed Studs Near a Free Edge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Lateral Blow out Failure of Headed Studs Near a Free Edge

Author(s): J. Furche and R. Eligehausen

Publication: Symposium Paper

Volume: 130

Issue:

Appears on pages(s): 235-252

Keywords: cover; embedment; failure mechanisms; loads (forces); studs; pullout tests; tension; Structural Research

DOI: 10.14359/1276

Date: 1/1/1992

Abstract:
Pullout tests with headed studs placed near a free edge have been carried out. In most of the tests, blow-out failure occurred. On the basis of this and other available test results, an empirical equation to calculate the failure load was derived. The equation takes into account the influence of the edge distance, the concrete strength, and the load-bearing area. The equation to calculate the failure load shows good agreement with the test results. The equation to calculate the critical edge distance at which the failure mode changes to steel rupture or to concrete cone failure is given. The values for critical edge distance are different from the values in ACI 349, Appendix B, because ACI 349 overestimates the concrete capacity for large edge distances.




  