Title: Superplasticized Cement Applications in Azerbaijan and Other States of the Former USSR
Author(s): Fuad A. Sultanov
Publication: Concrete International
Volume: 15
Issue: 4
Appears on pages(s): 48
Keywords:
DOI:
Date: 4/1/1993
Abstract: Powdered or granulated superplasticizers have recently come into use in Azerbaijan and other states of the former USSR as cement grinding aids.