Effects of Shrinkage and Temperature in Bonded Concrete Overlays

International Concrete Abstracts Portal

  


Title: Effects of Shrinkage and Temperature in Bonded Concrete Overlays

Author(s): Hak-Chul Shin and David A. Lange

Publication: Materials Journal

Volume: 101

Issue: 5

Appears on pages(s): 358-364

Keywords: bond strength; concrete; debonding; drying shrinkage; early ages of concrete; fiber-reinforced concrete; heat of hydration; overlay

DOI: 10.14359/13421

Date: 9/1/2004

Abstract:
Bonded concrete overlays are sometimes distressed by early age surface cracking and/or debonding of the interface between old and new concrete. This early age failure is mainly due to volume changes of the overlay concrete by shrinkage, thermal changes, and thermal gradients. To understand the early age behavior of bonded concrete overlays, extensive experimental measurements and numerical analysis were carried out. Laboratory overlay specimens were fabricated to measure opening displacement and debonding profiles at the interface. A finite element model was developed to assess debonding behavior due to volume changes. From the experimental measurements and numerical analysis, it was found that bonded concrete overlays with high-performance concrete (HPC) mixtures have a strong tendency toward early-age debonding. The main reason for this tendency is due to a high shrinkage gradient in the HPC mixtures and low bond strength at the interface.


ALSO AVAILABLE IN:

Electronic Materials Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer