Title: Reflections On Concrete Durability And On International Conferences On Concrete Durability

Author(s): K. and B. Mather

Publication: Symposium Paper

Volume: 223

Issue:

Appears on pages(s): 81-88

Keywords: concrete durability; concretes; exposure; specifications; variability

DOI: 10.14359/13496

Date: 10/1/2004

Abstract:
The Organizing Committee for this conference requested that we make some remarks and prepare some comments for inclusion in the Proceedings. These words are intended as a basis for the former and to serve as the latter. We observe that: Concrete is international; it is made locally; it has infinite variability; it can be made to be very uniform; and it can be made to last as long as you want it to. An unsolved problem is assessment of the nature and severity of the exposure, so that requirements can be graduated according to severity. Only when this problem is solved will we be able to stamp out specification overkill. The Organizing Committee also suggested we furnish biographical data and bibliographic data. The standard material accompanying this publication should suffice for the former. An appendix of selected items is provided for the latter purpose.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer