Title: A New Family of Latexes for Portland Cement

Author(s): Lou A. Kuhlmann

Publication: Symposium Paper

Volume: 166

Issue:

Appears on pages(s): 141-164

Keywords: latex; methyl methacrylate; permeability; polymer concrete; portland cement; styrene; temperature; Materials Research

DOI: 10.14359/1399

Date: 12/1/1996

Abstract:
A new family of latexes has been developed for use in portland cement that has a minimum film-formation temperature (MFFT) well above working temperature, eliminating the two major drawbacks of latex-modified mixtures: formation of a crust on the surface and difficulty in cleaning tools. Instead of coalescing to form a film, as do the typical latex modifiers for portland cement, these latex particles maintain their shape as spheres. Of the several formulations studied, two are reported here: a styrene polymer and a methyl methacrylate polymer, both carboxylated. In addition to extensive laboratory testing of both polymers, two field trials with the styrene latex formulation were conducted. These laboratory and field studies demonstrated that film formation is not necessary for latexes to contribute to the performance of portland cement mixes. The data from these studies are encouraging, but also revealed that much more work needs to be done to fully understand the capabilities and limitations of this family of latexes.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer