SP-030: Cracking, Deflection and Ultimate Load of Concrete Slab Systems

International Concrete Abstracts Portal

  


Title: SP-030: Cracking, Deflection and Ultimate Load of Concrete Slab Systems

Author(s): Editor: Edward G. Nawy

Publication: Symposium Paper

Volume: 30

Issue:

Appears on pages(s): 388

Keywords:

DOI: 10.14359/14083

Date: 1/1/1971

Abstract:
SP30 Specific recommendations are given in the sixteen papers contained in this volume, the majority of which were delivered at the International Symposium on the Cracking, Deflection, and Ultimate Load of Concrete Slab Systems held at the Annual ACI Convention in Denver, 1971. Containing the extensive works of twenty-nine international experts from five continents, the theme of this symposium volume is divided into three major areas: (1) serviceability as determined by crack control in one-way and two-way slab systems; (2) shear strength and moment transfer in column regions and concentrated load zones; (3) limit capacity of concrete slabs and plates, including membrane and arch action effects.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer