SP-038: Expansive Cement Concretes

International Concrete Abstracts Portal

  


Title: SP-038: Expansive Cement Concretes

Author(s): Editors: Milos Polivka and C. Taylor Test

Publication: Symposium Paper

Volume: 38

Issue:

Appears on pages(s): 504

Keywords:

DOI: 10.14359/14091

Date: 1/1/1973

Abstract:
SP38 A comprehensive study of the use of expansive cements and their effects on cracking in concrete. Covers research, design, field applications, and self-stressing. Contains 20 papers, including reports on use of expansive cement in walls, reinforced concrete pipe, pavements, grout, taxiways, and slabs.




  