Title: SP-181: Recent Developments in the Design and Specification of Concrete Paving Systems

Author(s): Editor: D.G. Zollinger / Sponsored by: ACI Committee 214 and ACI Committee 325

Publication: Symposium Paper

Volume: 181

Issue:

Appears on pages(s): 137

Keywords:

DOI: 10.14359/14174

Date: 3/1/1999

Abstract:
The six papers in this Symposium Publication address many different aspects of mechanistic design, such as environmental stress, improved pavement design methodology, approaches to performance-based specification, characterization of joint sealants for design purposes, characterization of concrete strength based on fracture properties, and others. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP181




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer