Title: The Forming Tolerance Cloud

Author(s): Dick Birley

Publication: Concrete International

Volume: 27

Issue: 10

Appears on pages(s): 52-54

Keywords: forming; reinforcing; tolerance; constructibility; placement

DOI:

Date: 10/1/2005

Abstract:
The series on constructibility issues continues with a look at tolerances for forming concrete and the conflicts that can arise when they are combined with tolerances for reinforcing bar fabrication and placement. These conflicts can be especially difficult to reconcile when they involve more than one trade, each within their own acceptable tolerances.




  