Title: Introduction to the State-of-the-Art Mat Foundation Design and Construction

Author(s): E. J. Ulrich, JR.

Publication: Symposium Paper

Volume: 152

Issue:

Appears on pages(s): 1-12

Keywords: mat foundations; soil mechanics; structural design; subgrades; Design

DOI: 10.14359/1519

Date: 3/1/1995

Abstract:
Subgrade response is the most important parameter in analyzing and designing mat foundations. Rational design of a mat foundation requires consideration of immediate and long term subgrade response. The soil response determines mat behavior, and differential movement exacerbates moments. Often, long term movement provides the most severe mat behavior characteristics. The popular use of a single modulus of subgrade reaction k, to model subgrade response is wrong and will lead to wrong designs. Mat analysis and design should be performed using the discrete area method, in which subgrade responses can be properly modeled because of the use of varying moduli of subgrade reaction. The geotechnical engineer and the structural engineer must form a solid bond to cope with mat foundation design from early planning through construction; both must work together to assure successful performance. Often, construction details and procedures will govern performance and can ruin any analysis. For this reason, the geotechnical engineer should be on site accessing conditions.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer