Title: Drying Concrete Brick to Take Out the Shrinkage
Author(s): L.E. Grube
Publication: Journal Proceedings
Volume: 24
Issue: 3
Appears on pages(s): 451-452
Keywords: none
DOI: 10.14359/15398
Date: 3/1/1928
Abstract: With the increasing necessity of late fall and early spring productions, we were confronted with a peculiar situation in the manufacture of concrete brick, that is, the drying of the brick after the steam cure process.