Title: Standard Specifications for Reinforced-Concrete Fence Posts

Author(s): ACI Committee on Specifications for Reinforced-Concrete Fence Posts

Publication: Journal Proceedings

Volume: 13

Issue: 2

Appears on pages(s): 468-470

Keywords: none

DOI: 10.14359/15918

Date: 2/1/1917

Abstract:
These specifications cover the manufacture of reinforced-concrete line posts made by hand processes or by machine.




  