Title: Report of Committee on Fireproofing and Insurance

Author(s): Edward T. Cairns, Chairman

Publication: Journal Proceedings

Volume: 3

Issue: 1

Appears on pages(s): 270-271

Keywords: none

DOI: 10.14359/16390

Date: 1/1/1907

Abstract:
The past year has witnessed some interesting progress in the development of fire resistance qualities of concrete.




  