Title: SP-236: Deformation Capacity and Shear Strength of Reinforced Conc Members Under Cyclic Loading

Author(s): Editors: Adolfo Matamoros and Kenneth Elwood / Sponsored by: Joint ACI-ASCE Committee 445 and Joint ACI-ASCE Committee 441

Publication: Symposium Paper

Volume: 236

Issue:

Appears on pages(s): 198

Keywords:

DOI: 10.14359/16443

Date: 5/26/2006

Abstract:
Earthquakes worldwide have clearly demonstrated the vulnerability of reinforced concrete members to degradation in shear strength when subjected to cyclic loading. Such degradation can lead to significant damage to the structure and, possibly, even collapse. With the advancement of performance-based earthquake engineering, where the response of the structure must be traced through all levels of damage, there is a significant need to accurately define the deformation capacity and shear strength for such members. This symposium publication represents an effort from researchers across the globe trying to address this challenging problem. Although at the time of publication there are some methodologies that can be used in performance-based earthquake engineering, there is a significant need for improved methods better suited for these types of applications. Furthermore, one of the concerns often expressed by researchers is that test data used in the past to develop and calibrate existing models consisted of relatively small data sets. This problem is compounded by differences between experimental studies in aspects such as the type of load history used, the manner in which deformations were recorded during tests, and the definition of displacement and strength at failure. The recent development of the PEER column database, hosted by the University of Washington, provided a valuable resource to overcome some of these problems. It presented researchers with a larger pool of data, which included the full hysteretic response of every column in the data set. Although this represented a very significant step forward, efforts of this kind should continue to improve the ability of researchers to calibrate and evaluate models for shear strength and deformation capacity. A joint technical session was organized by Joint ACI-ASCE Committees 441, Reinforced Concrete Columns, and 445, Shear and Torsion, during the American Concrete Institute’s Fall 2004 Convention in San Francisco, CA. The goal of the technical session was to showcase recent developments in this area, with the hope that continued discussion will lead to improved models that are suitable for performance-based engineering. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP236




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer