International Concrete Abstracts Portal

  


Title: Anchorage of Reinforcing Bars for Seismic Forces

Author(s): Neil M. Hawkins, I. Lin, and T. Ueda

Publication: Structural Journal

Volume: 84

Issue: 5

Appears on pages(s): 407-418

Keywords: anchorage (structural); beams (supports); columns (supports); bond (concrete to reinforcement); computer programs; connections; cyclic loads; earthquake-resistant structures; embedment; slippage; hooked reinforcement; mathematical models; reinforced conc

DOI: 10.14359/1651

Date: 9/1/1987

Abstract:
This paper describes a computer model that predicts load-attack end deformations and development length requirements for reinforcing bars anchored within exterior column-beam connections and subjected to inelastic reversed cyclic loadings typical of those


ALSO AVAILABLE IN:

Electronic Structural Journal



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.