Title: Concrete in Marine Enviroments
Author(s): Ivan L. Tyler
Publication: Symposium Paper
Volume: 8
Issue:
Appears on pages(s): 1-7
Keywords:
DOI: 10.14359/16645
Date: 1/1/1964
Abstract: The three main causes of deterioration in concrete, freezing and thawing, reinforcement corrosion, and chemical attack by sea water, are discussed on the basis of the fundamental concept that these causes can be generally minimized if watertight concrete is attained.