Title: Precast Concrete Wall Panels: Flexural Stiffness of Sandwich Panels

Author(s): D. W. Pfeifer and J. A. Hanson

Publication: Symposium Paper

Volume: 11

Issue:

Appears on pages(s): 67-86

Keywords:

DOI: 10.14359/16692

Date: 1/1/1965

Abstract:
Describes an investigation of the structural behavior of 31 cancrete sandwich panels tested under uniform flexural loading. Panel designs included different types of insulating core materials and different methods of providing positive shear connections between the reinforced concrete shells.




  