Title: Reinforced Concrete Columns: Effects of Lateral Tie Spacing on Ultimate Strength

Author(s): Fred M. Hudson

Publication: Symposium Paper

Volume: 13

Issue:

Appears on pages(s): 235-244

Keywords:

DOI: 10.14359/16762

Date: 1/1/1966

Abstract:
Sixty-four concrete columns were loaded to destruction to investigate the effects of tie spacing on ultimate strength. Variables included in the tests were column size, spacing of ties, strength of concrete, size of tie, percentage of longitudinal reinforcement, and position of load. Principal data obtained were failure loads, modes of failure, and strains.




  