Title: Small Scale Model Tests of Structural Components and Assemblies

Author(s): B. Wallace and H. Krawinkler

Publication: Symposium Paper

Volume: 84

Issue:

Appears on pages(s): 305-346

Keywords: beam-column frame; cyclic loads; earthquake resistant structures; failure; microconcretes; models; reinforced concrete; reinforcing steels; scale (ratio); shear walls; tests.

DOI: 10.14359/16898

Date: 10/1/1984

Abstract:
This paper presents the results of tests conducted on small-scale reinforced concrete models. Beam-column assemblies, an isolated shear wall, and a shear wall--frame unit were constructed to simulate portions of the full-scale test building at a scale of 1:12.5. Test results are used to determine the separate contributions of the wall, in-plane frame action, and transverse frame action in resisting lateral loads. Conclusions are drawn on the feasibility and limitations of small-scale model testing of reinforced concrete structures which are subjected to severe cyclic loading histories.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer