Title: Analysis of Cylindrical Shells and Folded Plates

Author(s): A.C. Scordelis

Publication: Symposium Paper

Volume: 28

Issue:

Appears on pages(s): 207-236

Keywords: computer programs; continuity (structural); cylindrical shells; edge beams; finite element method; folded plates; FORTRAN; prestressed concrete; reinforced concrete; shells (structural forms); stiffness methods; structural analysis

DOI: 10.14359/17159

Date: 1/1/1971

Abstract:
It is the purpose of this paper to present a "state of the art" discussion of the analysis of cylindrical shells and folded plates. Because these shell systems have been used widely during the past 30-40 years in reinforced concrete structures of all types, the literature on their analysis is very extensive.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.