Title: Predicition of Creep, Shrinkage, and Temperature Effects in Concrete Structure

Author(s): ACI Committee 209

Publication: Symposium Paper

Volume: 27

Issue:

Appears on pages(s): 51-94

Keywords: age; beams (supports); camber; composite construction (concrete to concrete); compressive strength; concrete slabs; concretes; cracking (fracturing); creep properties; curing; deflection; flat concrete plates; flexural strength; girders

DOI: 10.14359/17174

Date: 1/1/1971

Abstract:
This paper presents a review of methods for predicting creep, shrinkage and temperature effects in concrete structures as related to reinforced beams and one-way slabs, two-way construction, prestressed beams, and composite beams. The paper is generally consistent with the ACI Building Code (ACI 318-71) and includes material indicated in the Code, but not specifically defined therein.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer