Title: Performance Specifications for Durable Concrete

Author(s): John A. Bickley, R. Doug Hooton, and Kenneth C. Hover

Publication: Concrete International

Volume: 28

Issue: 9

Appears on pages(s): 51-57

Keywords: durability; exposure class; P2P initiative; performance specification; prescriptive specification

DOI:

Date: 9/1/2006

Abstract:
The ultimate goal of the Prescription-to-Performance initiative of the National Ready Mixed Concrete Association is to develop and encourage implementation of performance specifications, when appropriate, in the U.S. concrete industry. As part of this initiative, existing standards and specifications for concrete from several countries were reviewed. In this article, summaries of a couple of the relevant standards are provided, and initial steps for modifying common U.S. practice are proposed.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.