Time Dependent Deformations in a 70 Story Structure

International Concrete Abstracts Portal

  


Title: Time Dependent Deformations in a 70 Story Structure

Author(s): Donald W. Pfeifer, Donald D. Magura, Henry G. Russell, and W.G. Corley

Publication: Symposium Paper

Volume: 27

Issue:

Appears on pages(s): 159-186

Keywords: age; columns (supports); concretes; creep propertities; creep tests; deformation; differential shortening; drying shrinkage; field tests; Lake Point Tower; measuring instruments; moist curing; plain concrete; reinforced concrete; research; shearwalls

DOI: 10.14359/17181

Date: 1/1/1971

Abstract:
This report describes field and laboratory tests to determine instantaneous and time dependent deformations of the concrete columns and core walls in a 70 story reinforced concrete structure. These columns and core walls have different diameters and thicknesses over the height of the structure and are made with four different concretes.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer