Title: Anchor Bolts in Reinforced Concrete Foundations

Author(s): L. Elfgren, C. Broms, K. Cederwall, and K. Gylltoft

Publication: Symposium Paper

Volume: 103

Issue:

Appears on pages(s): 47-60

Keywords: anchor bolts; creep properties; cyclic loads; fatigue (materials); foundations; prestressing; reinforced concrete; shrinkage; Construction

DOI: 10.14359/1721

Date: 9/1/1987

Abstract:
Three areas of special interest to a designer are presented from a research project on anchor bolts. The areas are: a comparison between drilled holes and conical recesses; shrinkage and creep of grouts; and the positive influence of prestressing on bolts




  