The Analysis of Reinforced-Concrete Bridge Decks by the Line-Solution Technique

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Analysis of Reinforced-Concrete Bridge Decks by the Line-Solution Technique

Author(s): A. Coull and K.S. Rao

Publication: Symposium Paper

Volume: 23

Issue:

Appears on pages(s): 19-38

Keywords: bridge decks; bridges (structures); continuity (structural); deflection; elastic analysis (structural); matrix methods (structural); moments; reinforced concrete; shear; skew bridges; stresses; structural analysis

DOI: 10.14359/17226

Date: 1/1/1969

Abstract:
The object of this paper is to describe the use of the line-solution technique for the general analysis of complex bridge decks, which may be right, skew, or curved in plan.




  