Title: Conctraction of Cement, Expansion and Strength of Cement Mortar Caused by Heat Curing

Author(s): Roman Malinowski

Publication: Symposium Paper

Volume: 25

Issue:

Appears on pages(s): 251-274

Keywords: age; cement pastes; compressive strength; concretes; contraction; curing; expansion; mortars (material); research; temperature; thermal expansion; water-cement ratio

DOI: 10.14359/17339

Date: 1/1/1971

Abstract:
Volume changes due to thermal expansion, and the contraction as well as the strength of heat-cured cement mortar were studied.




  