Title: An Approach to the Control of Cracking in Reinforced Concrete

Author(s): Paul H. Kaar

Publication: Symposium Paper

Volume: 20

Issue:

Appears on pages(s): 141-158

Keywords:

DOI: 10.14359/17350

Date: 1/1/1968

Abstract:
A brief review of past research concerning crack control is presented and a recent investigation of similitude of top surface T-beam cracking under negative moment is described in detail. Similitude of cracking is evaluated in relation to the results of tests of quarter, half, and full-scale specimens. The reliability of expressions for computation of crack width is discussed.




  