Title: Ultimate Strength of Biaxiallt Eccentrically Loaded Concrete Columns Reinforced with High Strength Steel

Author(s): Peter D. Heimdahl and Albert C. Bianchini

Publication: Symposium Paper

Volume: 50

Issue:

Appears on pages(s): 93-118

Keywords: bixaxial loads; columns (supports); deformed reinforcement; eccentric loads; high strength steels; loads (forces); reinforced concrete; reinforcing steels; strains; stress-strain relationships; structural analysis; tensile strength; tied columns

DOI: 10.14359/17467

Date: 1/1/1975

Abstract:
The effect of using high strength reinforcement in square tied columns under uniaxially and biaxially eccentric loads is investigated.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer