Slenderness Effects in Reinforced Concrete Square Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Slenderness Effects in Reinforced Concrete Square Columns

Author(s): James Colville

Publication: Symposium Paper

Volume: 50

Issue:

Appears on pages(s): 165-192

Keywords: axial loads; bending moments; columns (supports); composite construction (concrete and steel, etc.); compressive strength; cracking (fracturing); displacement; eccentric loads; finite element method; loads (forces); modulus of elasticity; moments

DOI: 10.14359/17470

Date: 1/1/1975

Abstract:
The purpose of this work is to develop a simplified procedure for estimating the effects of tension cracking, nonlinearity of concrete in compression, yielding of the steel, and the effects of secondary bending on the displacements and moments in eccentrically loaded columns bent in single curvature.




  