International Concrete Abstracts Portal

  


Title: A New Approach to the Analysis of Cellular Bridge Decks

Author(s): bending; box beams; bridge decks; bridges (structures); deflection; deformation; models; prestressed concrete; reinforced concrete; shear properties; stresses; structural analysis; torsion

Publication: Symposium Paper

Volume: 35

Issue:

Appears on pages(s): 185-210

Keywords: bending; box beams; bridge decks; bridges (structures); deflection; deformation; models; prestressed concrete; reinforced concrete; shear propertiesp; stresses; structural analysis; torsion

DOI: 10.14359/17480

Date: 1/1/1973

Abstract:
Cellular concrete bridge decks have desirable aesthetic properties and because of their high torsional stiffness a good strength/weight ratio. Current analytical methods tend to use three dimensional models which are restricted in scope and are expensive.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer