Title: Code Criteria For Deflection Limitation in Reinforced Concrete Structures

Author(s): B.L. Meyers and G.M. Sabnis

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 1-14

Keywords: building codes; creep properties; deflection; flexural strength; loads (forces); reinforced concrete; shrinkage; span depth ratio; standards; stiffness

DOI: 10.14359/17504

Date: 1/1/1974

Abstract:
Code criteria for deflection limitation in reinforced concrete structures, from a number of countries, are reviewed and the two major methods used for deflection limitation are discussed. These methods are: limiting deflections to a fraction of the span length, and limiting the span-to-depth ratio.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer