Title: Variability of Deflections of Simply Supported Precast Prestressed Concrete Beams

Author(s): S. Zundelevich, H.S. Hamada, and A.N.L. Chiu

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 547-572

Keywords: beams (supports); coefficient of variation; creep properties; deflection; mix proportioning; modulus of elasticity; prestressed concrete

DOI: 10.14359/17525

Date: 1/1/1974

Abstract:
Methods for predicting the deflections of simply supported, non-composite and composite, prestresed concrete beams are presented.




  