Title: Model Techniques and Response Tests of Reinforced Concrete Structures Subjected to Blast Loads

Author(s): Norval Dobbs and Edward Cohen

Publication: Symposium Paper

Volume: 24

Issue:

Appears on pages(s): 407-448

Keywords:

DOI: 10.14359/17598

Date: 1/1/1970

Abstract:
Comparision of results of full-and model-scale explosive tests of cubicles and other similar reinforced concrete protective structures have shown that a reasonable estimate of the blast-resistant capabilities of these structures can be obtained from model tests as small as one-tenth scale. However, the results of the above tests have also indicated that care must be exercised in the preparation of the model and the test site as well as in the performance of the test in order to achieve the test data desired.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer