Title: Producing Architectural Concrete Using Plastic Form Liners and High Density Overlaid Plywoods

Author(s): Jerome H. Ford

Publication: Symposium Paper

Volume: 90

Issue:

Appears on pages(s): 9-22

Keywords: architectural concrete; chemical analysis; form liners; physical properties; plastics, polymers, and resins; plywood; General

DOI: 10.14359/1766

Date: 4/1/1986

Abstract:
The density of well-designed and compacted concrete directly reflects the density of the facing material of the formwork. Therefore, high-density plastics and high-density overlaid plywoods produce the most consistent concrete color, texture, and density over multiple uses providing a few do's and don'ts are considered. These do's and don'ts can be consolidated into the desire of all involved: designer, contractor and supplier, wanting to make it work and look good. All rules and regulations are worthless unless everyone involved wants to produce quality.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer